Seawater Valve Material Chart

Updated 2026-11-08 · Screening reference for engineers & contractors.

Direct answer · Seawater MOC orientation

For continuous seawater / brine, screen NAB (nickel aluminium bronze), duplex / super duplex, 254SMO (6Mo) and titanium — not default CF8M. Selection depends on velocity, temperature, stagnant vs flowing, chlorination, galvanic couples and owner class rules.

RFQ seawater valves — system · MOC family · size · class/PN · ends · qty.

Contact / RFQ WhatsApp

Material families (screening)

FamilyTypical gradesPREN / notesWhere it shows up
NABC95800 / ABS Type approval gradesCopper alloy — not PREN logicMarine firewater, seawater butterfly / check
DuplexF51 / A890 4A (S31803/S32205)PREN ≈ 35Offshore cooling, desal feed
Super duplexF53 / F55 / A890 5A–6APREN ≈ 40+Higher chloride / critical SW systems
6Mo / 254SMOUNS S31254 / similarHigh PREN austeniticDesal, high-chloride process
TitaniumGr.2 / Gr.5 wettedExcellent SW immunitySevere SW / heat exchanger loops
Ni-Cu (Monel family)M35-1 / N04400 familyGood SW; cost & galvanic careSelected marine / chemical
CF8M / 316A351 CF8M / F316Often inadequate for continuous SWShort exposure / splash only if approved

Duty orientation matrix

DutyCommon first pickEscalate toWatch-outs
Ship / platform firewaterNAB or duplexSuper duplexStagnation; coating of adjacent CS pipe
Seawater cooling (flowing)Duplex / NABSuper duplex / TiVelocity erosion-corrosion on Cu alloys
SWRO high-pressure brineSuper duplex / 254SMOTitaniumChlorides + pressure; crevices at seats
Desal low-pressure SWDuplex / NABSuper duplexBiofouling; chlorination chemistry
Ballast / bilge (marine)NAB / coated CS (if allowed)DuplexOwner + class society list
Heat exchanger SW sideTi / Cu-Ni / SDSSTiGalvanic couple with tube material
Chlorinated seawaterDuplex / SDSS / SMOTiFree chlorine residuals attack some alloys

Galvanic & system notes

IssueWhy it matters on valvesRFQ action
CS pipe + stainless valveGalvanic attack on carbon steelState insulation / coating / spool MOC
NAB + stainless fastenersCouple in wet SWSpecify compatible bolting / isolation
Crevice at wafer seatsLocalised pitting under gasket/seatPrefer resistant MOC; avoid stagnant traps
High velocityErosion of Cu alloysVelocity limit + duplex/Ti preference
“SS” only on BOQMay be read as CF8M — often wrongWrite duplex / NAB / SMO / Ti explicitly

Screening disclaimer: Seawater corrosion is system-specific (temperature, oxygen, chlorination, velocity, stagnant legs). This chart does not replace owner corrosion standards or class-society material lists. Confirm final MOC with the project corrosion engineer.

RFQ fields that unblock quoting

FieldWhy
Seawater / brine / firewaterSets corrosion family
Preferred MOC (NAB / duplex / SMO / Ti)Avoids CF8M default
Temperature · chlorination · velocity notesAlloy escalation
Valve type · size · Class/PN · endsConstruction
Class society / owner notesMarine compliance
Quantity + delivery portExport offer

FAQ

Is CF8M acceptable for seawater valves?

Often not for continuous seawater. 316/CF8M is prone to pitting and crevice corrosion in aerated seawater; prefer NAB, duplex, 254SMO or titanium per system design.

NAB or duplex for firewater?

Both appear on marine firewater specs. NAB is traditional for seawater valves; duplex is common on newer offshore lists. Follow the class society / owner material philosophy.

Can Supreme Valves quote seawater MOC valves?

Yes when media (seawater/brine), preferred family (NAB/duplex/SMO/Ti), size, rating and ends are stated on contact.html.

Related charts