Direct answer · Which body MOC?

WCB for non-corrosive process / steam within carbon-steel limits; CF8M (316SS cast) for mild corrosives and general chemical service; duplex / super duplex when chlorides, seawater or higher strength make austenitic stainless inadequate. Always pair body MOC with media, temperature, chloride and purchaser corrosion notes — not price alone.

RFQ from this chart — media · temp · size · class/PN · MOC · ends · qty.

Contact / RFQ WhatsApp

Material snapshot

GradeFamilyScreening temp bandStrength / costKey weakness
A216 WCBCarbon steel cast≈ −29 to 425 °CLowest cost · adequate strengthCorrosion / wet chlorides
A351 CF8M316 austenitic castCryo to ≈ 538 °C (trim/seat limit)Mid cost · good toughnessPitting / SCC in hot chlorides
Duplex (F51 / 4A)22Cr duplex≈ −50 to 250–300 °C*Higher strength · mid-high costUpper temp / phase stability
Super duplex (F53/F55)25Cr SDSSSimilar duplex band*Highest PREN · highest costFabrication / heat input control

*Duplex upper temperature is project-specific (often capped near 250–300 °C for continuous service). Confirm against purchaser corrosion standard.

Media × temperature selection matrix

Media / dutyAmbient–150 °C150–300 °C300–425 °C>425 °C
Clean hydrocarbon / dry gasWCBWCBWCB / WC6 reviewAlloy steel (WC6/WC9)
Steam / condensate (clean)WCBWCBWCB / WC6WC6 / WC9 / C12A
Utility / treated waterWCB or CF8MWCB / CF8MCF8M / alloyAlloy / SS per P-T
Seawater / brineDuplex / NAB / SMODuplex / SMO reviewSpecial alloysEngineer review
Chloride process waterCF8M caution → duplexDuplex preferredSpecial / Ni alloysEngineer review
Acids (dilute / general)CF8M / Alloy 20CF8M / specialtySpecialtySpecialty
CausticWCB / CF8M per conc.CF8M / Ni reviewNi alloys oftenEngineer review
Wet H₂S (sour)NACE WCB / SS / duplexNACE region tablesNACE + tempSpecial
Cryogenic LNG / N₂ / O₂LCB/LCC / CF8Mn/an/an/a
Firewater (marine)NAB / duplex / lined———

Decision rules used on RFQs

If…Then start with…Escalate when…
Non-corrosive oil/gas/steam, ambient–400 °CWCB body + stainless trim as neededWet CO₂, amines, acids, chlorides appear
Chemical / food / pharma wet serviceCF8M / CF3MHot chlorides, seawater, high PREN demand
Offshore / desal / SWRO / brineDuplex or NAB per systemHigh velocity + chlorides → super duplex / Ti
Cost pressure on water BOQWCB or DI + coating / SS discInternal corrosion history on sister units
Only “SS” written on MTOAsk CF8 vs CF8M; confirm chlorideSeawater listed — do not default CF8M

Trim note (body ≠ trim)

A WCB body with 13Cr or 316 trim is common. A CF8M body with hardfaced seats is common on dirty services. State body + trim + seat on the RFQ; do not assume “SS valve” means all-wetted stainless.

Screening disclaimer: This matrix is for early material orientation. Final MOC is set by corrosion engineering, ASME B16.34 P-T ratings, NACE/ISO 15156 where applicable, and the purchaser specification. Supreme Valves India quotes constructions by size, rating, MOC and ends.

RFQ fields that unblock quoting

FieldWhy
Media + chloride / H₂S / CO₂Chooses WCB vs CF8M vs duplex
Design / operating temperatureP-T and alloy band
Preferred body MOCWCB / CF8M / duplex grade
Trim / seat preferenceAvoids incomplete BOQ
Size · Class/PN · ends · qtyCommercial offer

FAQ

When is WCB enough instead of CF8M?

For non-corrosive hydrocarbons, steam and utility water within WCB temperature limits, carbon steel is usually the cost-effective body. Specify coating or stainless trim if external or seat corrosion is a concern.

When should duplex replace CF8M?

When chlorides, seawater, or higher strength at moderate temperature make 316/CF8M pitting or stress-corrosion risk unacceptable.

Can Supreme Valves quote WCB, CF8M and duplex valves?

Yes. Send media, design temperature, size, Class/PN, ends and preferred MOC via contact.html.

Related charts